Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 96.5 - 138 MPa | 14000 - 20000 psi | |
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 96.5 - 138 MPa | 14000 - 20000 psi | |
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 96.5 - 138 MPa | 14000 - 20000 psi | |
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 96.5 - 138 MPa | 14000 - 20000 psi | |
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |