Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 9.65 - 17.2 MPa | 1400 - 2500 psi | |
Dow SPECTRIM™ 35-S Reaction Moldable Polymer SPECTRIM™ 35-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information p.. |
|||
Injection Pressure | 9.65 - 17.2 MPa | 1400 - 2500 psi | |
Dow SPECTRIM™ 50-S Reaction Moldable Polymer SPECTRIM™ 50-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information p.. |