Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 82.7 - 172 MPa | 12000 - 25000 psi | |
PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 82.7 - 172 MPa | 12000 - 25000 psi | |
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 82.7 - 124 MPa | 12000 - 18000 psi | |
PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 82.7 MPa | 12000 psi | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |