Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 78.45 - 147.1 MPa | 11380 - 21340 psi | |
LG Chemical EG920 PMMA, General Purpose Grade for Extrusion General purpose grade with excellent stress cracking resistanceIntended mainly for exterior applicationsRecommended mainly for sheets, pipes, and profilesFeatures: Excellent transparency and eleganc.. |
|||
Injection Pressure | 78.45 - 147.1 MPa | 11380 - 21340 psi | |
LG Chemical EH910 PMMA, General Purpose Grade for Extrusion Excellent solvent resistanceHighest of all grades in heat resistance, mechanical strength, surface hardness and stress cracking resistanceFeatures: Excellent transparency and eleganceWeather resista.. |
|||
Injection Pressure | 78.45 - 147.1 MPa | 11380 - 21340 psi | |
LG Chemical IH830A PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |
|||
Injection Pressure | 78.45 - 147.1 MPa | 11380 - 21340 psi | |
LG Chemical IH830C PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |
|||
Injection Pressure | 78.45 - 147.1 MPa | 11380 - 21340 psi | |
LG Chemical IH830H PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® EH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® IG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL HG-3200 High Gloss Polypropylene, 20% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL HG-3250 High Gloss Polypropylene, 25% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL TE-5108 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Flow LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL TE-5202U Thermoplastic Elastomer Alloy, 20% Polymer Alloy, High Impact, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Injection Pressure | 78.45 - 88.26 MPa | 11380 - 12800 psi | Second |
LG Chemical LUPOS GP-2106F General Purpose ABS, 10% Glass Fiber Reinforced, Weather Resistant, Flame Retardant LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Injection Pressure | 78.45 - 88.26 MPa | 11380 - 12800 psi | Second |
LG Chemical LUPOS GP-2201F General Purpose ABS, 20% Glass Fiber Reinforced, Flame Retardant LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Injection Pressure | 78.45 - 88.26 MPa | 11380 - 12800 psi | Second |
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Injection Pressure | 78.45 - 88.26 MPa | 11380 - 12800 psi | Second |
LG Chemical LUPOS HR-2207 Heat Resistant SAN, 20% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Injection Pressure | 78.45 - 88.26 MPa | 11380 - 12800 psi | Second |
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL HF-3208H High Flow Polypropylene, 20% Mineral Fillers, General Purpose LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL HF-3308 High Flow Polypropylene, 30% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL HM-4354 Heat Resistant Polypropylene, 35% Glass Fiber/Mineral Filler Reinforced, High Strength, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL HM-5204B High Modulus Polypropylene, 20% Polymer Alloy, High Strength, High Flow, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL LW-4407 Low Warpage Polypropylene, 40% Glass Fiber/Mineral Filler Reinforced, Heat Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL TE-5005H Thermoplastic Elastomer Alloy, Dimensional Stability LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Injection Pressure | 78.45 - 98.07 MPa | 11380 - 14220 psi | Second |
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Injection Pressure | 78.45 - 88.26 MPa | 11380 - 12800 psi | Second |
LG Chemical LUPOS GP-2200H General Purpose ABS, 20% Glass Fiber Reinforced, High Heat Resistance LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Injection Pressure | 78.45 - 147.1 MPa | 11380 - 21340 psi | |
LG Chemical IH830 PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |