Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 110 - 138 MPa | 16000 - 20000 psi | |
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 152 MPa | 16000 - 22000 psi | |
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 110 - 138 MPa | 16000 - 20000 psi | |
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |