Polymer Property : Injection Pressure = 10000 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
Injection
Lubrizol Estane® 58070 Thermoplastic Polyurethane
Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr..
Injection Pressure 55.2 - 68.9 MPa
8000 - 10000 psi
Initial
Clariant Renol PCSP0019 Polycarbonate/Acrylic Alloy
Data provided by Clariant Masterbatches