Processing Properties Metric English Comments
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP 7645 Polycarbonate + PET, Impact Grade
Developmental productISO 7792-PC/PET,MHPR,-020(PC/PET)-blends, impact modifiedInjection molding gradeunreinforcedPreprocessingMax. Water content
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP 7665 Polycarbonate + PET, Mineral Filled Impact Grade
Developmental productISO 7792-1-PC/PET,MHPR,-030,MD20(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledPreprocessingMax. Water content
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch..
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP UT5005 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding gradeMakroblend DP UT5005* provides an outstanding balance of low-temperature impact strength and flowability beside e..
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP UT5007 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flow..
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP UT6000 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedinjection molding grade Makroblend DP UT6000* offers an exceptional low-temperature impact strength, good flowability and excellent chemical resis..
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP UT6003 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedUV-stabilizedinjection molding grade Makroblend DP UT6003* offers an exceptional low-temperature impact strength, good flowability and excellent c..
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch..
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® KU 2-7608 Polycarbonate + PBT, Mineral Filled Impact Grade
ISO 7792-1-PC/PBT,MHPR,-030,MD10(PC+PBT)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® KU 2-7609 Polycarbonate + PBT, Mineral Filled Impact Grade
ISO 7792-1-PC/PBT,MHPR,-030,MD20(PC+PBT)-blendsimpact modifiedInjection molding grade20% mineral filledPreprocessingMax. Water content
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® KU 2-7912/5 Polycarbonate + PBT, Impact Grade
Developmental productISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh flowhigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® KU 2-7915 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradeexcellent toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® S 7916 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing..
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® S 7916/2 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing..
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP 2-7655 Polycarbonate + PET, Mineral Filled Impact Grade
Developmental productISO 7792-1-PC/PET,MHPR,-030,MD10(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist..
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedPreprocessingMax. Water content
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® KU 2-7912/4 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP 6015 Polycarbonate + PBT
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade. Makroblend DP 6015* provides an outstanding balance of low-temperature impact strength and excellent chemical ..
Ejection Temperature 170 °C
338 °F
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT6007* offers an exceptional low-temperature impact strength, good flowability and..