Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 0.500 hour @Temperature 24.0 °C |
0.500 hour @Temperature 75.2 °F |
Tack Free |
Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding.. |
|||
Dry Time | 0.500 hour @Temperature 24.0 °C |
0.500 hour @Temperature 75.2 °F |
Tack Free |
Parker Chomerics CHO-SHIELD® 2044 Nickel-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2044 is an electrically conductive, one-component nickel-filled acrylic coating that is especially formulated for application on plastics to provide modest EMI shielding. C.. |