Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 274 - 335 °C | 525 - 635 °F | Average value: 304 °C Grade Count:8 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |