Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 228 °C | 442 °F | Film extrusion temperature |
Dow ATTANE™ 4213 Ultra Low Density Polyethylene ATTANE® 4213 copolymer is an ultra low density polyethylene that offers excellent flexibility, sealability, puncture resistance and superior strength. It exhibits oxygen transmission characteristic.. |
|||
Processing Temperature | 228 °C | 442 °F | Film extrusion temperature |
Dow ATTANE™ 4403 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4403 copolymer is an ultra low density polyethylene having high impact, tear strength and exceptional flexibility. It is designed for use in industrial/consumer blown film applications and .. |