Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 209 °C | 408 °F | Film extrusion temperature |
Dow AFFINITY™ PL 1880 Polyolefin Plastomer AFFINITY® PL 1880 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding packaging applications including high-speed, form-fill seal products. AFFINITY PL.. |
|||
Processing Temperature | 209 °C | 408 °F | Film extrusion temperature |
Dow DOWLEX™ 2101 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive a.. |
|||
Processing Temperature | 209 °C | 408 °F | Film extrusion temperature |