Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 349 - 382 °C | 660 - 720 °F | Average value: 373 °C Grade Count:14 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |