Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 274 - 335 °C | 525 - 635 °F | Average value: 304 °C Grade Count:8 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Processing Temperature | 274 - 293 °C | 525 - 560 °F | Average value: 286 °C Grade Count:52 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow AFFINITY™ HF 1030 Polyolefin Plastomer AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds,.. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow AFFINITY™ PL 1845 Polyolefin Plastomer Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow AFFINITY™ PL 1850 Polyolefin Plastomer AFFINITY® PL 1850 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistanc.. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli.. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food .. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good.. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2047A Polyethylene resin is a cast film polymer for high performance stretch cling applications. It provides outstanding tear strength, impact strength and toughness. It complies with U.S. .. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2247A Polyethylene resin is a cast film polymer for applications requiring outstanding tear strength, impact strength and toughness. This material complies with U.S. FDA Regulation 21 CFR 1.. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer Next Generation DOWLEX® NG 3347A resin with extra stretch performance (ESP)is an ethylene-octene-1 copolymer designed for cast stretch film applications such as industrial pallet wrap. DOWLEX NG 33.. |
|||
Processing Temperature | 274 °C | 525 °F | Film extrusion temperature |
Dow HDPE 05862N High Density Polyethylene Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |
|||
Processing Temperature | 274 - 293 °C | 525 - 560 °F | Average value: 284 °C Grade Count:9 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |