Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 232 - 272 °C | 450 - 522 °F | |
Nylene® 826 Nylon Copolymer Dry as molded. Nylene 826 is a special nylon copolymer suitable for both blown and cast film co-extrusion. Nylene 826 has a lower melt point and is less crystalline than standard nylon 6 resins. In.. |
|||
Processing Temperature | 232 - 272 °C | 450 - 522 °F | |
Nylene® CX3395 Nylon Copolymer Dry as molded. Nylene CX3395 is a higher RV version of 826 which is a special nylon copolymer suitable for both blown and cast film co-extrusion. Nylene CX3395 has a lower melt point and is less cr.. |