Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 94.0 °C | 201 °F | Seal initiation temperature |
Dow AFFINITY™ PL 1850 Polyolefin Plastomer AFFINITY® PL 1850 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistanc.. |