Polymer Property : Processing Temperature = 199 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 93.0 - 204 °C
199 - 399 °F
DuPont Teijin Films Mylar® 854 Polyester Packaging Film, 60 Gauge
Data provided by DuPont Packaging Polymers.DuPont Melinex® DuPont Melinex® 854 is a clear, one side coextruded heat sealable surface similar to Melinex® 850. The opposite surface is adhesion pret..
Processing Temperature 93.0 - 160 °C
199 - 320 °F
Average value: 139 °C Grade Count:11
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..
Processing Temperature 93.0 - 121 °C
199 - 250 °F
Mold temperature
Quantum Composites QC-8151C 55% Glass Fiber Vinyl Ester Static-Dissipative SMC  (discontinued **)
QC-8151C is a vinyl ester sheet molding compound (SMC) designed for compression molding components requiring dimensional stability, resistance to high temperatures plus sufficient electrical conduct..