Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 171 - 179 °C | 340 - 355 °F | Suggested Extusion Stock |
S&E Specialty Polymers TufFlex™ GA-5330D PVC/PU Compound Application: 105°C, matte finish, flame retardant PVC/PU jacketing material designed for retractile cord applications.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 174 - 179 °C | 345 - 355 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ G-3489 PVC Compound Application: A general purpose PVC based flexible compound designed for profile extrusion.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 168 - 179 °C | 335 - 355 °F | Recommended Stock Temperature |
Sylvin Technologies 6400-85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 168 - 179 °C | 335 - 355 °F | Recommended Stock Temperature |
Sylvin Technologies 7056 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 168 - 179 °C | 335 - 355 °F | Recommended Stock Temperature |
Sylvin Technologies 503 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 168 - 179 °C | 335 - 355 °F | Recommended Stock Temperature |
Sylvin Technologies 6034-85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 168 - 179 °C | 335 - 355 °F | Recommended Stock Temperature |
Sylvin Technologies 6034-85 UV PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 168 - 179 °C | 335 - 355 °F | Recommended Stock Temperature |
Sylvin Technologies 6112-85 FU PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 168 - 179 °C | 335 - 355 °F | Recommended Stock Temperature |
Sylvin Technologies 6137-85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 168 - 179 °C | 335 - 355 °F | Recommended Stock Temperature |
Sylvin Technologies 6147-83 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |