Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 48.0 - 55.0 °C @Time 576 sec |
118 - 131 °F @Time 0.160 hour |
Immersion |
Henkel Turco Altrex 24 Cleaner Turco Altrex 24 is an inhibited, non-etching, concentrated liquid alkaline cleaner for cleaning aluminum and aluminum alloys. The product is an effective remover of most soils found on aluminum, plu.. |
|||
Processing Temperature | 40.0 - 55.0 °C | 104 - 131 °F | Tacking Temperature |
Aquabond Technologies Aquabond™ ABS-55 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Processing Temperature | 40.0 - 55.0 °C | 104 - 131 °F | Tacking Temperature |
Aquabond Technologies Aquabond™ ABS-65 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |