Processing Properties Metric English Comments
Processing Temperature 1052 °C
1925 °F
fusing temperature
Wall Colmonoy COLMONOY® 4 - Hard-Surfacing Alloy With Chromium Boride
Description: Contains wear-resistant chromium borides and carbides. Has greater impact resistance and workability than Colmonoy No.5. Finished with carbide tools and grinding.Method of Application..
Processing Temperature 1052 °C
1925 °F
fusing temperature
Wall Colmonoy COLMONOY® 22 - Nickel Alloy With Tungsten Carbide
Description and Application: A harder version of Colmonoy 23A and 24, for similar applications. Can be finished with a file.Method of Application: Oxyacetylene, FusewelderInformation provided by Wa..