Thermal Properties Metric English Comments
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM E968
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers.
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM E968
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM E968
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers.
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF)
Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Solef® 20808 Polyvinylidene Fluoride (PVDF)
Copolymer; Low ViscosityAdditional Properties: Abrasion Resistance - ASTM D4060 29.0 mg; Coefficient of Friction - ASTM D1894 0.280; Coefficient of Linear Thermal Expansion - ASTM D696 1.4E-4 to 1.6..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF)
Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM ..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 25.0 °C
0.382 BTU/lb-°F

@Temperature 77.0 °F
solid; DSC
Eastman Eastman AP005 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 25.0 °C
0.382 BTU/lb-°F

@Temperature 77.0 °F
solid; DSC
Eastman Eastman AP006 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 25.0 °C
0.382 BTU/lb-°F

@Temperature 77.0 °F
solid; DSC
Eastman Eastman AP007 Copolyester
Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM E968
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM E968
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers.
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM E968
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers.
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.