Polymer Property : Specific Heat Capacity = 1.08 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.08 J/g-°C

@Temperature 800 °C
0.258 BTU/lb-°F

@Temperature 1470 °F
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation
Microtherm® Moulded Pipe Sections (MPS) are preformed pieces of pipe insulation designed to provide a thermally efficient insulation system for piping of all sizes from 25 mm (1”) upwards. F..