Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, 1.6 mm sheet Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, 12.7-50.8 mm bar Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 316°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 982°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, all-weld metal, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, mill annealed Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, plate, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.573 J/g-°C @Temperature 600 °C |
0.137 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Ultimet® alloy, plate, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.572 J/g-°C @Temperature 500 °C |
0.137 BTU/lb-°F @Temperature 932 °F |
|
Special Metals INCOLOY® alloy 832 Stainless Steel INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula.. |
|||
Specific Heat Capacity | 0.574 J/g-°C @Temperature 500 °C |
0.137 BTU/lb-°F @Temperature 932 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |