Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.544 J/g-°C @Temperature 93.3 °C |
0.130 BTU/lb-°F @Temperature 200 °F |
|
Zircar Zirconia ZYK-15 Zirconia Cloth Insulation Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexibl.. |
|||
Specific Heat Capacity | 0.544 J/g-°C @Temperature 93.3 °C |
0.130 BTU/lb-°F @Temperature 200 °F |
|
Zircar Zirconia ZYW-15 Zirconia Cloth Insulation Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, 1.6 mm sheet Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 316°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, mill annealed Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, plate, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.545 J/g-°C @Temperature 500 °C |
0.130 BTU/lb-°F @Temperature 932 °F |
|
Haynes Ultimet® alloy, plate, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Specific Heat Capacity | 0.544 J/g-°C @Temperature 93.3 °C |
0.130 BTU/lb-°F @Temperature 200 °F |
|
Zircar Zirconia ZYF-150 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Specific Heat Capacity | 0.544 J/g-°C @Temperature 93.3 °C |
0.130 BTU/lb-°F @Temperature 200 °F |
|
Zircar Zirconia ZYF-50 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Specific Heat Capacity | 0.544 J/g-°C @Temperature 93.3 °C |
0.130 BTU/lb-°F @Temperature 200 °F |
|
Zircar Zirconia ZYW-15 Zirconia Cloth Insulation Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo.. |
|||
Specific Heat Capacity | 0.544 J/g-°C @Temperature 93.3 °C |
0.130 BTU/lb-°F @Temperature 200 °F |
|
Zircar Zirconia ZYW-30A Zirconia Cloth Insulation Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo.. |
|||
Specific Heat Capacity | 0.544 J/g-°C @Temperature 93.3 °C |
0.130 BTU/lb-°F @Temperature 200 °F |
|
Zircar Zirconia ZYF-150 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Specific Heat Capacity | 0.544 J/g-°C @Temperature 93.3 °C |
0.130 BTU/lb-°F @Temperature 200 °F |
|
Zircar Zirconia ZYF-50 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Specific Heat Capacity | 0.544 J/g-°C @Temperature 93.3 °C |
0.130 BTU/lb-°F @Temperature 200 °F |
|
Zircar Zirconia ZYW-30A Zirconia Cloth Insulation Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo.. |