Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 150 - 250 °C
88.9 µin/in-°F

@Temperature 302 - 482 °F
ASTM E831
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st..
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 55.0 - 100 °C
88.9 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 55.0 - 100 °C
88.9 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 127UV BK701 Acetal Homopolymer  (Unverified Data**)
Delrin® 127UV BK701 is a high viscosity, UV stabilized acetal homopolymer. It has excellent impact strength, UV resistance and thermal stability. It is well suited for automotive interior applicati..
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 55.0 - 100 °C
88.9 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 300CP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance.Information provided by DuPont Perf..
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 55.0 - 100 °C
88.9 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 527UV BK701 Acetal Homopolymer  (Unverified Data**)
Delrin® 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvements in UV aging characteristics and ther..
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 55.0 - 100 °C
88.9 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p..
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 100 - 250 °C
88.9 µin/in-°F

@Temperature 212 - 482 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig..
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 55.0 - 100 °C
88.9 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer
Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a..
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 55.0 - 100 °C
88.9 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer
Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic..
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 55.0 - 100 °C
88.9 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer
Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro..
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 55.0 - 100 °C
88.9 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100TL is a high viscosity acetal homopolymer, containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.Inform..
CTE, linear, Transverse to Flow 160 µm/m-°C

@Temperature 23.0 - 80.0 °C
88.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East)
VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin.