CTE, linear, Transverse to Flow 82.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
CTE, linear, Transverse to Flow 82.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific)
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
CTE, linear, Transverse to Flow 82.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Europe-Africa-Middle East)
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
Copyright © lookpolymers.com All Rights Reserved