Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Asia Pacific) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Europe-Africa-Middle East) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
43.9 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 150 °C |
43.9 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 150 °C |
43.9 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
43.9 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Asia Pacific) >PPE+PA66-I-TD10 |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East) >PPE+PA66-I-TD10 |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific) Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. .. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific) Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. .. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
43.9 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ3001 PBT Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS high gloss Noryl |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Asia Pacific) high gloss Noryl |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Asia Pacific) high gloss Noryl |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Europe-Africa-Middle East) high gloss Noryl |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |