Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 78.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® OQ3820 PC High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
CTE, linear, Transverse to Flow | 78.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® OQ3820 PC (Asia Pacific) High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
CTE, linear, Transverse to Flow | 78.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® OQ3820 PC (Europe-Africa-Middle East) High Viscosity, UV-stabilized grade for ophthalmic lenses. |