Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific) Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 9945A PC Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 9945A PC (Asia Pacific) Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 9945A PC (Europe-Africa-Middle East) Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7652 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Medium flow, excellent low temperature ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® OQ1060 PC Copolymer Optical quality, high flow, high purity Polycarbonate copolymer resin with reduced oxygen transmission for advanced DVD applications such as Limited Play DVD.This data was supplied by SABIC-IP for t.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DL002PC PC LNP* LUBRICOMP* DL002PC is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this grade are: Wear Resistant, Exceptional Processing, Clean Compound System. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 100 - 150 °C |
40.6 µin/in-°F @Temperature 212 - 302 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12 LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific .. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific .. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific) LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa.. |