Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific) Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7672 PC (Asia Pacific) Non FR PC + GF, UV-Stabilizer, balanced flow & impact. Available in Opaque only. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7672 PC (Asia Pacific) Non FR PC + GF, UV-Stabilizer, balanced flow & impact. Available in Opaque only. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7681 PC Copolymer (Asia Pacific) Polycarbonate with high flow, good processability, good impact and thermal properties, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited translucent colors onl.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7681 PC Copolymer (Asia Pacific) Polycarbonate with high flow, good processability, good impact and thermal properties, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited translucent colors onl.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX WX94736 PBT LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xylex X8419 PC+POLYESTER Low-medium flow, suitable for blow molding, injection molding, extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Asia Pacific) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Europe-Africa-Middle East) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |