Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CM6240 PC+ABS (Asia Pacific)
CYCOLOY CM6240 resin is a flame retardant PC/ABS blend featuring balanced properties of high modulus, good flow and ductility. It is of Br- & Cl-free flame retardant systems intended to meet thin wa..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX NS0031 PC+ABS (Asia Pacific)
Faradex NS0031 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel. Added features of this material include: EMI/RFI Shiel..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East)
CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature 100 - 200 °C
35.6 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® BR111BL is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical proper..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature 0.000 - 100 °C
35.6 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DD000P PC
LNP* STAT-KON* DD000P is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Electrically Conductive, Exceptional Processing.
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DD000P PC (Asia Pacific)
LNP* Stat-kon* DD000P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing.
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature 50.0 - 100 °C
35.6 µin/in-°F

@Temperature 122 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4870HH PC+PET
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific)
LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X5630 PC+PET
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP
LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity.
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature 100 - 200 °C
35.6 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® BR111 is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical ..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific)
LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based ..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East)
LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East)
LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC
LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing 20% Glass Bead, 15% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retard..
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON MFD02 PP
LNP* STAT-KON* MFD02 is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific)
LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications