Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 55.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
31.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF PX06417 PA 6 LNP THERMOTUF* PX06417 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |