Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 53.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC LNP THERMOCOMP* DF004ER is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. Mold Release. |
|||
CTE, linear, Transverse to Flow | 53.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
CTE, linear, Transverse to Flow | 53.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
CTE, linear, Transverse to Flow | 53.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific) LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 53.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific) LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 53.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific) LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 53.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RV00CES PA 66 LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
CTE, linear, Transverse to Flow | 53.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
CTE, linear, Transverse to Flow | 53.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific) LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 53.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |