Polymer Property : CTE, linear, Transverse to Flow = 53.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific)
LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS
LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East)
LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific)
LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopolymer
LNP* LUBRICOMP* KP003AXZ is a compound based on Acetal Homopolymer resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66
LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific)
LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS
LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific)
LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL HN731A PPE+PS
PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine..
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL 731 PPE+PS
PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi..
CTE, linear, Transverse to Flow 95.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL 731 PPE+PS
PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi..