Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 93.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG34LG ABS
Automotive: Low gloss ABS for unpainted interior applications.
CTE, linear, Transverse to Flow 93.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® MG34LG ABS
Automotive: Low gloss ABS for unpainted interior applications.
CTE, linear, Transverse to Flow 93.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG34LGHF ABS
Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 93.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® MG34LGHF ABS
Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 93.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS
LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 93.6 µm/m-°C

@Temperature 25.6 - 149 °C
52.0 µin/in-°F

@Temperature 78.0 - 300 °F
Diameter
Saint-Gobain Rulon® 488 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Transverse to Flow 93.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10
LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Flame Retardant..
CTE, linear, Transverse to Flow 93.6 µm/m-°C

@Temperature 25.6 - 149 °C
52.0 µin/in-°F

@Temperature 78.0 - 300 °F
Diameter
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f..