Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 160 - 250 °C |
51.1 µin/in-°F @Temperature 320 - 482 °F |
|
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
51.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG511DP is a medium viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications such .. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
51.1 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
51.1 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
51.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
51.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
51.1 µin/in-°F @Temperature 73.4 - 131 °F |
ASTM E 831 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 100 - 200 °C |
51.1 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Chevron Phillips Xtel® XK2040 Polyphenylene Sulfide Alloy
(discontinued **) Natural Color Polyphenylene Sulfide AlloyXtel™ XK2040 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties alo.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
51.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 100 - 200 °C |
51.1 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Chevron Phillips Xtel® XK2140 Polyphenylene Sulfide Alloy
(discontinued **) Black Polyphenylene Sulfide AlloyXtel™ XK2140 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties along with .. |