Polymer Property : CTE, linear, Transverse to Flow = 49.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS
LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS
LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific)
LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature 25.6 - 149 °C
49.0 µin/in-°F

@Temperature 78.0 - 300 °F
Diameter
Saint-Gobain Rulon® W2 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA6.10
LNP THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA6.10
LNP THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11
LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA 6/10 (Asia Pacific)
LNP* THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA 6/10 (Asia Pacific)
LNP* THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature 25.6 - 93.3 °C
49.0 µin/in-°F

@Temperature 78.0 - 200 °F
Diameter
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f..