Polymer Property : CTE, linear, Transverse to Flow = 47.8 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 86.0 µm/m-°C

@Temperature 55.0 - 160 °C
47.8 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan..
CTE, linear, Transverse to Flow 86.0 µm/m-°C

@Temperature 0.000 - 100 °C
47.8 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM E831
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhi..
CTE, linear, Transverse to Flow 86.0 µm/m-°C

@Temperature 0.000 - 100 °C
47.8 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material ..
CTE, linear, Transverse to Flow 86.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly
LNP* THERMOCOMP* KFB11 is a compound based on Acetal Copolymer resin containing 5% Glass Fiber, 5% Glass Bead. Added features of this material include: Low Warpage, Chemically Coupled.
CTE, linear, Transverse to Flow 86.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East)
Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release.
CTE, linear, Transverse to Flow 86.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
47.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA
Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to ..
CTE, linear, Transverse to Flow 86.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
47.8 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
CTE, linear, Transverse to Flow 86.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
47.8 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East)
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
CTE, linear, Transverse to Flow 86.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KFB11 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled.