Polymer Property : CTE, linear, Transverse to Flow = 41.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature 0.000 - 100 °C
22.8 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM E228
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)  (discontinued **)
Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature 20.0 °C
22.8 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4-230NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compare..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature 20.0 °C
22.8 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4-230BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compared to oth..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature -20.0 - 150 °C
22.8 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 2310F PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature 23.0 - 150 °C
22.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2310F PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2300 PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP ..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature -20.0 - 150 °C
22.8 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM HU2310 PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature 23.0 - 150 °C
22.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2310 PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature -20.0 - 150 °C
22.8 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM HU2310 PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature 23.0 - 150 °C
22.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2310 PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature -20.0 - 150 °C
22.8 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM HU2310 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature 23.0 - 150 °C
22.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2310 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DX05474 PC
LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold ..
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific)
LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret..