CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12
LNP* LUBRICOMP* IFL34 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IFL34 is a compound based on Nylon 6/12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66
LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -20.0 - 150 °C
22.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM UC1200 PEI (Asia Pacific)
12% carbon fiber reinforced Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 listing in recognized colors.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ..
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific)
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P..
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -20.0 - 150 °C
22.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI
LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -20.0 - 150 °C
22.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI (Europe-Africa-Middle East)
LNP* Stat-kon* Ultem_UC1200 compound is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10
LNP* THERMOCOMP* QF0069 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP UC006H PPA
LNP THERMOCOMP* UC006H is a compound based on Polyphthalamide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS (Asia Pacific)
LNP* Thermocomp* ZF0049 is a compound based on PPE+PS Blend resin containing Flame Retardant. Added features of this material include: Flame Retardant.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched
LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6
LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat.
CTE, linear, Transverse to Flow 39.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS
LNP* THERMOCOMP* ZF0049 is a compound based on PPE+PS resin containing 20% Glass Fiber. Added feature of this material is: Flame Retardant.