Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 51.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DDF029 PC LNP STAT-KON* DDF029 is a compound based on Polycarbonate resin containing Carbon, Glass Fiber. Added features of this material include: Electrically Conductive. Flame Retardant. |