Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 47.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 47.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 47.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Asia Pacific)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 47.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Asia Pacific)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 47.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 47.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.