Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 36.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU
LNP THERMOCOMP* GF006 is a compound based on Polysulfone resin containing 30% Glass Fiber.
CTE, linear, Transverse to Flow 36.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU
LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber.
CTE, linear, Transverse to Flow 36.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon DX96690 PC
LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America..