Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON MS000IL PP LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c.. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON MS000IL PP LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c.. |