Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer
LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer
LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -40.0 - 95.0 °C
63.3 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Valox® V4860HR PBT
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® VIC4311 PBT
VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings.
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VIC4311 PBT
VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings.
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -40.0 - 95.0 °C
63.3 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific)
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -40.0 - 95.0 °C
63.3 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East)
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.