Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer
LNP LUBRICOMP* KL004 is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer
LNP LUBRICOMP* KL004 is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* Fu..
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* Fu..
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KL004 is a compound based on Acetal Copolymer containing PTFE. Added features include Internally Lubricated.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KL004 is a compound based on Acetal Copolymer containing PTFE. Added features include Internally Lubricated.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer
LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer
LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004U is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* F..
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004U is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* F..
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer (Asia Pacific)
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer (Asia Pacific)
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific)
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific)
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal
LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal
LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare.
CTE, linear, Transverse to Flow 111 µm/m-°C

@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL WCV072 PPE+PP