Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG34LG ABS Automotive: Low gloss ABS for unpainted interior applications. |
|||
CTE, linear, Parallel to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® MG34LG ABS Automotive: Low gloss ABS for unpainted interior applications. |
|||
CTE, linear, Parallel to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG34LGHF ABS Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® MG34LGHF ABS Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 (Asia Pacific) LNP* Lubricomp* RP004 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |