Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific)
Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11
LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing 25% Glass Fiber, 10% Graphite. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific)
LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific)
LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific)
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PKN4775 PPE+PS
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL PKN4775 PPE+PS
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..