Polymer Property : CTE, linear, Parallel to Flow = 69.6 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 69.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
CTE, linear, Parallel to Flow 69.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific)
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
CTE, linear, Parallel to Flow 69.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer
Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce..
CTE, linear, Parallel to Flow 69.6 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXM141R PC
FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color ..
CTE, linear, Parallel to Flow 69.6 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East)
FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color ..
CTE, linear, Parallel to Flow 69.6 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXM141R PC (Asia Pacific)
FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color ..