Polymer Property : CTE, linear, Parallel to Flow = 60.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 108 µm/m-°C

@Temperature 25.6 - 93.3 °C
60.0 µin/in-°F

@Temperature 78.0 - 200 °F
Length
Saint-Gobain Rulon® W2 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Parallel to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly
LNP* THERMOCOMP* KFB11 is a compound based on Acetal Copolymer resin containing 5% Glass Fiber, 5% Glass Bead. Added features of this material include: Low Warpage, Chemically Coupled.
CTE, linear, Parallel to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KFB11 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled.