Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 57.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS (Asia Pacific) LNP* Thermocomp* ZF0049 is a compound based on PPE+PS Blend resin containing Flame Retardant. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS LNP* THERMOCOMP* ZF0049 is a compound based on PPE+PS resin containing 20% Glass Fiber. Added feature of this material is: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific) LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |